NANO-CRYSTALLINE COMMON MODE CHOKE CORE
Nanocrystaline ribbon yog cov khoom siv sib nqus hlau nplaum uas muaj qhov loj me (~ 10nm) uas yog tsim los ntawm Fe, Si, B, Cu, Nb thiab lwm yam, thiab tau txais los ntawm cov txheej txheem tshwj xeeb annealing ntawm qhov cua txias ntawm 10 degree / s.6.
NanocrystallineribbonyogtusmosSib nqusalloy khoom nrogsuperfinenplejloj (~ 10nm) uas yog tsim los ntawm tus Fe, Si, B, Ua,Nb thiab lwm yam element, thiab tau dhauspecfic annealing txheej txheem ntawm txias tus nqi ntawm 10degree / s.6
Qhov zoo tshaj plaws ntawm cov khoom siv hlau tshiab no yog cov txheej txheem tsim khoom luv luv, tsim los ntawm ib-kauj ruam thiab txuag lub zog noj. crystalline alloy, yog li nws muaj peev xwm txaus siab rau qhov kev ua tau zoo ntawm kev ua haujlwm siab thiab poob qis. Cov khoom siv no tsuas yog siv rau hauv kev tsim cov high-end hom chokes, siab zaus transformer, txhua yam ntawm tam sim no transformers thiab high-end magnetic ampliier, thiab lwm yam cores thiab Cheebtsam yog tsuas yog siv nyob rau hauv tshiab zog tsheb fais fab kev tswj system, tsav tsheb. qhov system, wireless charging module rau lub xov tooj ntawm tes, kev tsheb ciav hlau, lub zog nag lossis daus, daim phiaj-txuas nrog photovoltaic inverter, cov khoom siv hluav taws xob digital, thiab cov ntsuas ntse hauv daim phiaj hluav taws xob kom tau raws li qhov yuav tsum tau muaj ntawm qhov siab, tam sim no loj, miniaturization thiab txuag hluav taws xob.
NANO-CRYSTALLINE COMMON MODE CHOKE CORE
Daim ntawv thov
Inverter Circuit Court
Zaus converter
UPS
Hloov hom Fais fab
EMC lim

Yam ntxwv
High saturate induction - txo qhov ntim ntawm CMC
Zoo heev impedance zaus yam ntxwv
Muaj peev xwm tiv taus qhov tsis sib xws tam sim no

Zoo kub stability
SQ COMMON MODE SERIES CORE
Yam ntxwv
Zoo dua EMI kev tawm tsam
Flat hlau ntsug winding tswv yim tuaj yeem txais yuav, nrog tsis tshua muaj peev xwm faib tawm thiab zoo dua cov cua sov dissipation
Zam kev ua haujlwm tsis zoo los ntawm kev ntxhov siab ntawm lub hauv paus
Lub hauv paus ntsiab lus ua haujlwm ntawm hom hom inductor
Thaum cov tam sim no ib txwm ntws los ntawm hom hom inductor nyob rau hauv Circuit Court, tam sim no yuav tsim rov qab magnetic teb nyob rau hauv tib theem winding inductor kauj kom tshem tawm ib leeg. Lub sijhawm no, qhov inductance yog kwv yees li xoom thiab qhov impedance rau cov khoom siv tam sim no tsawg heev.
Thaum lub kauj dhau los ntawm lub kauj, hom hom tam sim no yuav raug txo kom tsawg, thiab lub kauj yuav tsim ib hom hom tam sim no.
Yog li ntawd, qhov loj dua qhov impedance ntawm hom hom inductor, qhov zoo dua cov hom kev lim dej. Hauv qee qhov ntau zaus, cov ntaub ntawv nanocrystalline muaj impedance siab dua li cov khoom siv ferrite. Piv nrog rau ferrite, qhov pib permeability ntawm nanocrystals yog ntau dua, yog li qhov ntim tuaj yeem me dua, cov winding coils tsawg dua, qhov kev faib tawm me me, thiab cov yam ntxwv impedance zoo dua.
|
Sunbow Part No. |
Core qhov ntev |
Ua tiav core dimensions |
Ua tau zoo hla ntu |
Txhais txoj kev ntev |
Permeability (ntawm 10KHZ) |
AL Nominal Tus nqi** |
||
|
OD × ID × HT |
OD × ID × HT |
AFe |
lFe |
Tus nqi luv |
Refer nce tus nqi |
10 kHz |
100 kHz |
|
|
mm |
mm |
cm2 ua |
cm |
μH |
μH |
|||
|
SWB 120805 Stb |
Φ12×8×5 |
Φ14.3×6.8×6.9 |
0.08 |
3.1 |
50000-120000 |
90000 |
28 |
6.7 |
|
SWB-151005 |
Φ15×10×5 |
Φ17.1×8.3×7.1 |
0.09 |
3.9 |
50000-120000 |
91000 |
29 |
6.8 |
|
SWB-CM201208 |
Φ20×12.5×8 |
Φ22.6×10.3×10.2 |
0.24 |
5.1 |
50000-120000 |
97000 |
56 |
14 |
|
SWB-CM201210 |
Φ20×12×10 |
Φ22.6×10.5×12.5 |
0.31 |
5 |
50000-120000 |
85000 |
62 |
15 |
|
SW-WM 211510 |
Φ21×15×10 |
Φ23.5×13.1×12.3 |
0.23 |
5.7 |
50000-120000 |
85000 |
43.5 |
9.2 |
|
SWB-CM252065 |
Φ25×20×6.5 |
Φ26.8×18.7×7.9 |
0.12 |
7.1 |
50000-120000 |
80000 |
17.1 |
3.8 |
|
SW-CM25 2010 |
Φ25×20×10 |
Φ28×17.2×13.2 |
0.2 |
7.1 |
50000-120000 |
80000 |
28 |
7.2 |
|
SWB 251610 Stb |
Φ25×16×10 |
Φ28×14×13.1 |
0.35 |
6.4 |
50000-120000 |
90000 |
67 |
15 |
|
SWB 261610 Stb |
Φ26×16×10 |
Φ28.3×14×12.8 |
0.39 |
6.6 |
50000-120000 |
90000 |
57 |
14 |
|
SWB 302010 |
Φ30×20×10 |
Φ33.2×17.8×13.3 |
0.39 |
7.9 |
50000-120000 |
90000 |
60 |
14 |
|
SWB-CM302015 |
Φ30×20×15 |
Φ33.6×17.8×17.2 |
0.59 |
7.9 |
50000-120000 |
96000 |
88 |
20 |
|
SWB-CM322010 |
Φ32×20×10 |
Φ34.4×18.1×13 |
0.47 |
8.2 |
50000-120000 |
95000 |
57 |
14 |
|
SWB 402515 Stb |
Φ40×25×15 |
Φ44.5×21.8×18.8 |
0.88 |
10.2 |
50000-120000 |
94000 |
99 |
23 |
|
SWB 403215 Stb |
Φ40×32×15 |
Φ44.5×29×19 |
0.47 |
11.3 |
50000-120000 |
90000 |
48 |
11 |
|
SWB-CM453015 |
Φ45×30×15 |
Φ48.3×26.4×18.2 |
0.88 |
11.8 |
50000-120000 |
95000 |
87 |
20 |
|
SWB-503215 |
Φ50×32×15 |
Φ53.8×28.5×18.2 |
1.4 |
12.9 |
50000-120000 |
90000 |
100 |
27 |
|
SWB-CM504020 |
Φ50×40×20 |
Φ53.6×37×23.2 |
0.78 |
14.1 |
50000-120000 |
80000 |
45 |
14 |
|
SWB 635025 Stb |
Φ63×50×25 |
Φ69×46×29 |
1.27 |
17.7 |
50000-120000 |
90000 |
59 |
18 |
|
SWB 644020 Stb |
Φ64×40×20 |
Φ68.2×37×23.5 |
1.87 |
16.3 |
50000-120000 |
90000 |
115 |
29 |
|
SWB-CM805020 |
Φ80×50×20 |
Φ83.8×46.6×24.8 |
2.34 |
20.4 |
50000-120000 |
95000 |
94 |
28 |
|
SWB 9060200000 |
Φ90×60×20 |
Φ95.4×55×24.5 |
2.34 |
23.6 |
50000-120000 |
90000 |
90 |
25 |
|
SWB 1027625 Stb |
Φ102×76×25 |
Φ107×70.3×29.7 |
2.54 |
27.9 |
50000-120000 |
95000 |
91 |
22 |
Lus Cim: Cov lus saum toj no tsuas yog sau qee yam khoom. Cov kev qhia tshwj xeeb thiab kev ua haujlwm ntawm nanocrystalline core tuaj yeem kho raws li cov neeg siv khoom xav tau. Thov hu rau peb kom paub meej.
Cim npe nrov: nano-crystalline hom choke core, Tuam Tshoj nano-crystalline hom choke core manufacturers, lwm tus neeg, Hoobkas