Nanocrystalline Ribbon

Nanocrystalline Ribbon

Fe-raws li Amorphous sawb yog ib qho tshiab mos magnetic alloy. Nws yog tsim los ntawm cov thev naus laus zis thev naus laus zis ntawm kev sib zog sai ntawm cov hlau molten ntawm qhov txias ntawm ib lab degree / sec. Thaum lub sij hawm tus txheej txheem no cov hlau yog sai quenched raws li ib daim ntawv ntawm ribbon nrog 25-35 µm thickness, thiab cov micro-structure ntawm cov hlau yog cov amorphous vim lub siab quenching tus nqi.

Alloys thiab Specification

 

Fe-base nanocrystalline alloy ribbon (tsuas yog tsim los ntawm Fe, Cu, Nb, Si, B) yog qhov poob qis heev nrog siab permeability.

Fe-raws li Amorphous sawb yog ib qho tshiab mos magnetic alloy. Nws yog tsim los ntawm cov thev naus laus zis thev naus laus zis ntawm kev sib zog sai ntawm cov hlau molten ntawm qhov txias ntawm ib lab degree / sec. Thaum lub sij hawm tus txheej txheem no cov hlau yog sai quenched raws li ib daim ntawv ntawm ribbon nrog 25-35 µm thickness, thiab cov micro-structure ntawm cov hlau yog cov amorphous vim lub siab quenching tus nqi.

Nws muab kev ua tau zoo heev rau tam sim no transformer, EMC / EMI, Invent transformer thiab lwm yam.

 

Daim ntawv thov:

 

●EMC hom cores,

●Differential hom lim cores

● Fais fab tam sim no transformer cores.

● High precision tam sim no transformer cores.

● Zero sequence tam sim no transformer cores

● Hybrid tam sim no transformer cores

●Magnetic amplifier cores, mem tes killer cores, Saturated inductor cores

 

Kev sib xyaw

Fe: 70%, Si: 11%, B: 9%, Nb+Cu: Sib npaug

 

Main Khoom

Tsawg coercivity -1.5 A / m Siab hluav taws xob tiv taus -0.9 μΩ.m

 

Daim ntawv thov

High-frequency Transformer, Tam sim no Transformer, Hom Hom Choke (CMC)…

 

Magnetic Properties (tus nqi raug)

Kev quab yuam

1.5

A/m

Curie kub

570

degree

Saturation flux ceev

1.23

T

Qhov siab tshaj plaws permeability

200,000

 

Pib permeability

80,000

 

Saturation magnetostriction

<1

ppm ua

 

Static Virgin Curve (tus nqi raug)

Sib nqus teb zog

H (A/m)

1

4

10

150

500

1000

Induction

B (T)

0.1

1.0

1.02

1.1

1.2

1.23

 

Hlau Loss-B=0.1T (tus nqi raug)

Thickness

d (mm)

30

30

30

30

30

30

Ntau zaus

f (KHz)

17

20

40

60

80

100

Poob

p (W / kg)

0.2

0.27

0.9

1.8

3.0

4.5

 

Lub cev khoom

Qhov ntom

7.25

g/cm3

Hluav taws xob resistivity

0.9

μΩ.m

Thermal expansional

7.6

ppm / degree

Crystallization kub

510

degree

 

Daim ntawv(soft & bendable)

·Cold-rolled:

Thickness =26 ~ 34μm

Dav =50/80mm

·Slitting-strip:

Thickness =26 ~ 34μm

Dav =5 ~ 50mm

 

Lus Cim Tseem Ceeb:

Cov khoom sib nqus tshwj xeeb tuaj yeem raug cuam tshuam los ntawm kev kho cua sov.

Yuav kom ua tiav cov khoom zoo, qhov kawg annealing yog qhov tseem ceeb!

 

Peb kauj ruam los pib koj qhov kev hloov kho hnub no!

 

Qhia peb seb koj xav tau dab tsi

Peb muab nanocrystaline Soft Sib Nqus Khoom & Amorphous Soft Sib Nqus Khoom, thov qhia koj cov ntaub ntawv thov:

1. Khoom siv

2.Application - Tam sim no Transformer, CMC, Suab, thiab lwm yam?

3.Strips dav

4.Srips Thickness --µm?

5.Potential Quantity -- kg?

 

Tau txais kev daws teeb meem & nqe lus

Peb yuav ua haujlwm ntawm qhov kev daws teeb meem zoo tshaj plaws thiab muab cov lus qhia tshwj xeeb & nqe lus rau koj qhov kev tshuaj xyuas.

 

Qauv ntau lawm thiab ntau lawm

Peb yuav pib ntau lawm tom qab cov neeg siv khoom paub meej thiab validation ntawm cov qauv.

 

Pob:

 

product-1200-820

 

peb lub rooj cob qhia

 

our workshop

 

peb cov khoom siv

 

our equipment1

our equipment2

 

peb qhov kev sim

 

our testing1

our testing2

 

peb daim ntawv pov thawj

 

our certification

 

peb cov txheej txheem ntau lawm

 

our production process

 

peb exhibition

 

page-1200-1200

 

Cim npe nrov: nanocrystalline ribbon, Tuam Tshoj nanocrystalline ribbon manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

(0/10)

clearall