Peb ib txwm tham txog amorphous motors, tab sis vim li cas nanocrystalline motors tsis tshua tau txais?

news-954-720

Nws paub zoo tias silicon steel yog cov khoom siv tseem ceeb rau stator cores ntawm amorphous motors, ua raws li cov khoom siv amorphous trending. Technically hais, cov khoom hierarchy mus:nanocrystalline> amorphous> silicon steel. Yog li vim li cas cov khoom siv nanocrystalline tsis haum rau lub cev muaj zog?

 

Nov yog cov ntaub ntawv siv tau sib piv ntawm peb cov ntaub ntawv:

1. Sib nqus Flux ceev

Silicon hlau> Amorphous alloy> Nanocrystalline alloy

  • Silicon steel: kwv yees . 1.7-2.0T
  • Amorphous alloy: kwv yees li . 1.4-1.6T
  • Nanocrystalline alloy: kwv yees . 1.25T

 

2. Fais fab zaus Core poob

Nanocrystalline alloy < Amorphous alloy < Silicon hlau

  • Qhov tsis muaj -load core poob ntawm amorphous cores tsuas yog 1/6 ntawm silicon steel cores ntawm lub zog zaus.
  • Qhov tsis muaj -load core poob ntawm nanocrystalline cores tsuas yog 1/4 ntawm amorphous cores nyob rau hauv tib yam mob.

 

3. Kev kub siab ruaj khov

Silicon hlau> Nanocrystalline alloy> Amorphous alloy

  • Curie kub ntawm silicon steel: nyob ib ncig ntawm 700 degree
  • Curie kub ntawm nanocrystalline alloy: nyob ib ncig ntawm 570 degree
  • Curie kub ntawm amorphous alloy: nyob ib ncig ntawm 400 degree

 

4. Kev ua haujlwm nyuaj

Silicon steel < Amorphous alloy < Nanocrystalline alloy

  • Silicon steel nta zoo toughness thiab yooj yim rau stamping txoj kev.
  • Amorphous ribbons yog nkig thiab nyuaj rau stamp.
  • Nanocrystalline ribbons yog qhov yooj yim dua thiab tsis siv rau stamping.

 

5. Tus nqi ntau lawm

Nanocrystalline alloy> Amorphous alloy> Silicon hlau

  • Silicon steel: tsuas yog ob peb txhiab RMB ib tuj
  • Amorphous alloy: tshaj kaum txhiab RMB ib tuj
  • Nanocrystalline alloy: 40,000 txog 50,000 RMB ib tuj

Los ntawm tsib- qhov sib piv cov ntaub ntawv saum toj no, nws yog qhov tseeb tias silicon steel tseem yog qhov kev xaiv zoo tshaj plaws rau kev ua haujlwm dav dav, siab - cov khoom siv hluav taws xob thiab tus nqi- siv tau zoo.

Cov ntaub ntawv Amorphous tau dhau los ua qhov kev xaiv zoo tshaj plaws rau kev lag luam hluav taws xob tshiab rau ib qho laj thawj yooj yim: tam sim no tsuas yog cov khoom siv sib nqus zoo tshaj plaws uas yogcoj mus muag siv tau, tus nqi -txuag thiab efficiency- txhim kho.

Txawm hais tias cov ntaub ntawv nanocrystalline khav theeb qhov zoo tshaj plaws - zaus poob kev ua haujlwm, lawv qhov tsis tshua muaj qhov sib nqus sib nqus flux ntom ntom thiab cov nqi tsim khoom ntau dhau ua rau lawv ua tsis tau zoo rau kev tsim cov tub ntxhais hauv lub cev tam sim no.